COMPARATIVE ANALYSIS OF FAILURE MECHANISMS UNDER TENSILE IMPACT FATIGUE AND CONVENTIONAL LOW-CYCLE FATIGUE FOR A100 STEEL

  • Aiming at the typical fatigue failure problem induced by repeated cyclic impacts during the takeoff and landing processes of carrier-based aircraft, this study investigates the fatigue performance and damage mechanism of A100 ultra-high strength steel under repeated tensile impact loads and conventional low-cycle fatigue loads. A scientific research method combining macroscopic experimental testing and microscopic microstructure analysis is fully adopted in this work. Based on the drop-weight impact testing machine, a dedicated compression-to-tension conversion fixture and matched tensile impact fatigue specimens are independently designed and fabricated. Systematic impact fatigue tests under three different impact energy levels are carried out on smooth A100 steel specimens. The dynamic impact load-time history curves, real strain response of specimen test sections and fatigue life data of all tested samples are accurately acquired. Furthermore, according to the loading characteristics of tensile impact fatigue, a set of comparative conventional fatigue test schemes is reasonably formulated. Conventional low-cycle fatigue tests with three different strain levels are completed for comparative analysis.The experimental results indicate that under the condition of consistent maximum load levels, the impact fatigue life of A100 steel is significantly shorter than its conventional low-cycle fatigue life, and the impact fatigue data exhibits relatively large dispersion. Finally, optical microscopy (OM) and scanning electron microscopy (SEM) were employed to characterize the fracture surfaces of specimens. It is found that both types of fatigue fractures consist of crack initiation zone, propagation zone and shear lip zone. Nevertheless, cracks in conventional low-cycle fatigue mostly initiate at the specimen surface with stable crack growth, dominated by progressive damage accumulation. In contrast, cracks under tensile impact fatigue tend to initiate inside the material. The transient impact effect induces simultaneous nucleation and rapid propagation of multiple microcracks, leading to more pronounced brittle fracture features. The research conclusions provide a reliable and important technical reference for the structural design and engineering analysis of A100 ultra-high strength steel components serving under complex impact fatigue load conditions.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return