A100材料拉伸冲击疲劳与常规低周疲劳失效机理对比分析
COMPARATIVE ANALYSIS OF FAILURE MECHANISMS UNDER TENSILE IMPACT FATIGUE AND CONVENTIONAL LOW-CYCLE FATIGUE FOR A100 STEEL
-
摘要: 针对舰载机起降过程中存在多次冲击导致的疲劳失效问题, 采用实验测试和微观分析相结合的方法研究了A100材料在重复拉伸冲击载荷和常规低周疲劳载荷下的疲劳性能和损伤机理. 基于落锤冲击实验机, 自行设计了一套压缩转拉伸专用夹具和拉伸冲击疲劳试样, 针对A100材料的光滑试样, 开展了3种能量下的冲击疲劳实验, 获得了冲击载荷-时间历程、试样实验段的实际应变响应和试样疲劳寿命; 进而, 根据拉伸冲击疲劳载荷特点, 设计了与之对比的常规疲劳实验, 并开展了3种应变水平的常规低周疲劳实验. 结果表明, 在最大载荷水平一致的条件下, 冲击疲劳寿命远小于常规低周疲劳寿命, 并且呈现出较大的分散性. 最后, 利用光学显微镜(Optical Microscopy, OM)与扫描电子显微镜(Scanning Electron Microscopy, SEM)对试样断口开展观测. 发现两类疲劳断口均包含裂纹源区、扩展区与剪切唇区, 但常规低周疲劳裂纹多萌生于试样表面, 裂纹扩展平稳, 以渐进式损伤累积为主; 而拉伸冲击疲劳裂纹更易在材料内部萌生, 冲击瞬态效应诱发多微裂纹同步萌生与快速扩展, 脆性断裂特征更突出. 研究结果为A100超高强钢结构件在受冲击疲劳载荷作用下的设计分析提供了重要参考.Abstract: Aiming at the typical fatigue failure problem induced by repeated cyclic impacts during the takeoff and landing processes of carrier-based aircraft, this study investigates the fatigue performance and damage mechanism of A100 ultra-high strength steel under repeated tensile impact loads and conventional low-cycle fatigue loads. A scientific research method combining macroscopic experimental testing and microscopic microstructure analysis is fully adopted in this work. Based on the drop-weight impact testing machine, a dedicated compression-to-tension conversion fixture and matched tensile impact fatigue specimens are independently designed and fabricated. Systematic impact fatigue tests under three different impact energy levels are carried out on smooth A100 steel specimens. The dynamic impact load-time history curves, real strain response of specimen test sections and fatigue life data of all tested samples are accurately acquired. Furthermore, according to the loading characteristics of tensile impact fatigue, a set of comparative conventional fatigue test schemes is reasonably formulated. Conventional low-cycle fatigue tests with three different strain levels are completed for comparative analysis.The experimental results indicate that under the condition of consistent maximum load levels, the impact fatigue life of A100 steel is significantly shorter than its conventional low-cycle fatigue life, and the impact fatigue data exhibits relatively large dispersion. Finally, optical microscopy (OM) and scanning electron microscopy (SEM) were employed to characterize the fracture surfaces of specimens. It is found that both types of fatigue fractures consist of crack initiation zone, propagation zone and shear lip zone. Nevertheless, cracks in conventional low-cycle fatigue mostly initiate at the specimen surface with stable crack growth, dominated by progressive damage accumulation. In contrast, cracks under tensile impact fatigue tend to initiate inside the material. The transient impact effect induces simultaneous nucleation and rapid propagation of multiple microcracks, leading to more pronounced brittle fracture features. The research conclusions provide a reliable and important technical reference for the structural design and engineering analysis of A100 ultra-high strength steel components serving under complex impact fatigue load conditions.
下载: